Zero-delamination engineering through rigorous mechanical profiling
CSP 3-5
Surface Profile Target
>400 PSI
Tensile Bond Strength
100%
Elcometer Verification
Shot-blast profiling
Moisture mitigation
Broadcast build matrix
Topcoat seal
Mechanical surface preparation via abrasive blast equipment to achieve nominal CSP 3 to 5 anchor profile, removing laitance and weak concrete paste.
In-situ relative humidity and calcium chloride testing to verify vapor emission levels before epoxy primer anchoring.
Rapid-cure polyaspartic or chemical-resistant urethane topcoat application ensuring 24-hour return to heavy industrial service.
Multi-layer aggregate broadcast and high-build epoxy or polyurea layering to achieve specified mil-thickness ratings.
On-site verification metrics
6,000+
PSI Concrete Minimum
3.0 mm
Nominal System Thickness
24 HR
Full Chemical Cure
Schedule an on-site concrete core moisture test
Our technical team deploys directly to Michigan facilities to execute pull-tests and relative humidity assessments before bidding.